شدت بازی
Strong base
ساختار فیزیکی
macroporous
Strong Acid Cation
Gel
macroporous
کاربردها
Organic ScavengerSugar decolorizationWater demineralization (deionization)
Chromatography - SugarFructose Enrichment
polishing mixed bedspolishing mixed beds Non-regenerableprimary mixed beds after reverse osmosis RegenerableRegenerable
ideally when treating water with: – High oxidant level – High temperature on the cation resin Mixed bed polishingSystems requiring exceptionally high osmotic stability Condensate polishing Demineralization
ساختار شیمیایی
Macroporous polyacrylic crosslinked with divinylbenzene (DVB)
ویژگی ظاهری
spherical beadsWhite opaque
گروه عاملی
Quaternary amine type I (Trimethylamine)
Sulfonic acid
Sulfonic acid
فرم یونی
Cl-
Calcium form
H+
H +
نگهداری رطوبت (Moisture Retention)
65-72
60 - 63 %
45.0 – 51.0%
52.0 – 58.0%
اندازه ذرات (Particle Size µm)
0.315-1.25 mm≥95
-
≤ 1.20
800 ± 100
uncracked(%)
≥96
وزن حمل و نقل (Shipping weight g/L)
0.65-0.73
750 - 790
817
755
Specific gravity (g/ml)
1.04-1.10
Effective size (mm)
0.4 - 0.6
ضریب یکنواختی ذرات (Uniformity coefficient)
<1.7
Reversible swelling
Free base → Cl- (%) <20
حداکثر دمای کارکرد
80 ℃
120
5 – 60°C (41 – 140°F)
5 – 150°C (41 – 302°F)
محدوده pH
0-12
-
0 – 14
0 – 14
flow rate
8-40 BV/h
Regenrant
2-10% NaCl2-6% NaOH
ظرفیت تبادل یونی (Capacity)
1.5
≥ 2.00
≥ 1.70
جرم ذرات (Particle density g/mL)
-
وزن حمل و نقل (Shipping weight lbs/ft3)
46.9 - 49.4
ضریب یکنواختی
-
≤ 1.20